Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3EG3 GR32257 - PA6-GF15 - BASF

Material Data Center offers the following functions for Ultramid® B3EG3 GR32257:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Glass fiber reinforced injection moulding grade for housings (e.g: automotive mirror housings).
Also used for wheels of mountain bikes.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 65 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 0.4 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.7 / * % ISO 294-4, 2577
Ejection temperature 150 °C -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 5900 / 2900 MPa ISO 527
Stress at break 120 / 65 MPa ISO 527
Strain at break 5 / 19 % ISO 527
Charpy impact strength, +23°C 40 / 115 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 39 / 42 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 5.5 / 12 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 4.3 / 4 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 220 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 195 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 215 / * °C ISO 75-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Yellow Card available yes / * - -
Other propertiesdry / condUnitTest Standard
Water absorption 8.1 / * % Sim. to ISO 62
Humidity absorption 2.5 / * % Sim. to ISO 62
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 150 / * cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 280 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Lubricants, Release agent
Special Characteristics
Heat stabilized or stable to heat
Applications
Automotive, Sports Equipment
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 270 - 290 °C
injection molding, Melt temperature, recommended: 280 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.